| Performance | Unit | Parameter | 
| Component | Wt% | 94.6%ZrO2,5.2%Y2O3 | 
| Filled Density | Kg/l | 3.5(φ5mm) | 
| Density | g/cm3 | 5.95-6.00 | 
| Hardness | GPa | >11 | 
| Elasticity Modulus | GPa | 200 | 
| Thermal conductivity | W/m.k | 3 | 
| Coefficient of thermal Expansion | 10*10-6/℃(20-400) | 9.6 | 
| Crush Strength | Kg.f | >160(φ2mm) | 
| Bending toughness | MPam1/2 | 8 | 
| Size | 0.1-0.2 0.2-0.3 0.3-0.4 0.4-0.6 0.6-0.8 0.8-1.01.0-1.2 1.2-1.4 1.4-1.6 1.6-1.8 1.8-2.0 2.0-2.2...................50 | |
 
		    
			It is especially suitable for vertical stirring mills, horizontal rolling ball mills, vibration mills and various rod-pin sand mills with high linear speed. Finely dispersed and ground. The application areas are as follows:
1. Wear-resistant and corrosion-resistant products: coatings, textiles, pigments, printing and dyeing.
2. High-strength, high-toughness products: magnetic materials, piezoelectric ceramics, dielectric ceramics.
3. Prevent pollution: medicine, food, cosmetics.
4. Ceramics: electronic ceramics, refractory ceramics, structural ceramics.